MIG Wire; Filler Metal 0.03 Percent Carbon/1 to 2.5 Percent Manganese/0.65 to 1 Percent Silicon/0.03 Percent Phosphorus/0.03 Percent Sulfur/18 to 20 Percent Chromium/11 to 14 Percent Nickel/0.75 Percent Copper/2 to 3 Percent Molybdenum; Diameter 0.045 Inch; Metal Used On 316 and 316L Stainless Steel; Packaging Type Steel Spool; Approval AWS A5.9, ASME SFA-A5.9, CWB/CSA W48-06, ISO 14343-B; Shielding Gas 90 Percent Hydrazine/7.5 Percent Argon/2.5 Percent Carbon Dioxide (Short Circuiting Transfer), 98 Percent Argon/Balance Oxygen Dioxide or Carbon Dioxide (Axial Spray Transfer); Tensile Strength 81 KSI; Yield Strength 59 KSI; Elongation 40 Percent; Application Semiautomatic Welding, Molybdenum Bearing Austenitic Stainless Steel
Engineered Surface Treatment for Weldability Control in Semiautomatic Applications; High Silicon Level for Increased Puddle Fluidity and Toe Wetting; Molybdenum Grade for Increased Corrosion Resistance
Approval: | AWS A5.9, ASME SFA-A5.9, CWB/CSA W48-06, ISO 14343-B |
Diameter: | 0.045 Inch |
Filler Metal: | 0.03 Percent Carbon/1 to 2.5 Percent Manganese/0.65 to 1 Percent Silicon/0.03 Percent Phosphorus/0.03 Percent Sulfur/18 to 20 Percent Chromium/11 to 14 Percent Nickel/0.75 Percent Copper/2 to 3 Percent Molybdenum |
Metal Used On: | 316 and 316L Stainless Steel |
Packaging Type: | Steel Spool |
Prices and stock availability subject to change, and may differ by location; Items may include unforeseen shipping and/or tariffs; Taxes where applicable; Shipping limited to company market area which includes select regions of Iowa, Illinois and Missouri.
Please call for details.