MIG Welding Wire; Filler Metal 0.4 Percent Molybdenum/1.69 Percent Manganese/0.63 Percent Silicon/0.011 Percent Sulfur/0.17 Percent Copper; Diameter 0.045 Inch; Packaging Type Spool; Approval CAN/CSA-ISO14341, B-G 55A 3 G4M31 (ER80S-D2), CSA W48, MIL-E-23765/2, 80S-3; Wire Composition 0.01 Percent Phosphorous, 1.69 Percent Manganese, 0.17 Percent Copper, 0.08 Percent Carbon, 0.011 Percent Sulfur, 0.63 Percent Silicon, 0.09 Percent Nickel; Yield Strength 95 KSI (98 Percent Argon, 2 Percent Oxygen), 77 KSI (100 Percent Carbon Dioxide); Tensile Strength 110 KSI (98 Percent Argon, 2 Percent Oxygen), 92 KSI (100 Percent Carbon Dioxide); Elongation 22 Percent (98 Percent Argon, 2 Percent Oxygen), 23 Percent (100 Percent Carbon Dioxide); Testing Temperature Rating -20 Deg F (98 Percent Argon, 2 Percent Oxygen, 100 Percent Carbon Dioxide); Welding Process GMAW (MIG/MAG); Application Industrial and General Fabrication, Mobile Equipment, Automotive, Ship/Barge Building
Approval: | CAN/CSA-ISO14341, B-G 55A 3 G4M31 (ER80S-D2), CSA W48, MIL-E-23765/2, 80S-3 |
Diameter: | 0.045 Inch |
Filler Metal: | 0.4 Percent Molybdenum/1.69 Percent Manganese/0.63 Percent Silicon/0.011 Percent Sulfur/0.17 Percent Copper |
Packaging Type: | Spool |
Prices and stock availability subject to change, and may differ by location; Items may include unforeseen shipping and/or tariffs; Taxes where applicable; Shipping limited to company market area which includes select regions of Iowa, Illinois and Missouri.
Please call for details.