Bare Wire; Filler Metal 0.02 Percent Carbon, 3 Percent Manganese, 0.41 Percent Silicon, 0.007 Percent Phosphorus, 0.003 Percent Sulphur, 70.5 Percent Nickel, 20.5 Percent Chromium, 0.009 Percent Copper, 0.4 Percent Iron, 0.05 Percent Aluminum, 0.3 Percent Titanium, 0.012 Percent Cobalt; Diameter 0.035 Inch; Metal Used On Nickel Alloy; Packaging Type Spool; Approval AWS/ASME SFA 5.14; Voltage Rating 17 to 20 Volt; Current Rating 70 to 90 Amp; Tensile Strength 85000 PSI; Yield Strength 52000 PSI
This Alloy can also be used for Dissimilar Welding using Various Nickel Alloys to Stainless Steels or Carbon Steel, as well as for Overlaying Carbon Steels; Also Used for Welding 9% Nickel Steel to One another having High Impact Strength at Low Temperature; This Versatile Alloy has High Strength and Good Corrosion Resistance, with Oxidation Resistance and Creep-Rupture Strength at Elevated Temperature
Approval: | AWS/ASME SFA 5.14 |
Diameter: | 0.035 Inch |
Filler Metal: | 0.02 Percent Carbon, 3 Percent Manganese, 0.41 Percent Silicon, 0.007 Percent Phosphorus, 0.003 Percent Sulphur, 70.5 Percent Nickel, 20.5 Percent Chromium, 0.009 Percent Copper, 0.4 Percent Iron, 0.05 Percent Aluminum, 0.3 Percent Titanium, 0.012 Percent |
Metal Used On: | Nickel Alloy |
Packaging Type: | Spool |
Prices and stock availability subject to change, and may differ by location; Items may include unforeseen shipping and/or tariffs; Taxes where applicable; Shipping limited to company market area which includes select regions of Iowa, Illinois and Missouri.
Please call for details.